找词语>英语词典>abrade翻译和用法

abrade

英 [əˈbreɪd]

美 [əˈbreɪd]

v.  磨损(岩石等); 擦伤(皮肤等)

过去分词:abraded 过去式:abraded 现在分词:abrading 第三人称单数:abrades 

GRE医学

BNC.34653 / COCA.28660

牛津词典

    verb

    • 磨损(岩石等);擦伤(皮肤等)
      to rub the surface of sth, such as rock or skin, and damage it or make it rough

      柯林斯词典

      • VERB 磨损;磨蚀;擦伤
        Toabradesomething means to scrape or wear down its surface by rubbing it.
        1. My skin was abraded and very tender.
          我擦破皮了,一碰就疼。

      英英释义

      verb

      双语例句

      • The injury after falling has smaller cut, abrade and more severe loss, the coxa ministry fracture that if cause functional activity commonly, is damaged badly.
        跌倒后的损伤有较轻的划伤、擦伤和更严重的损伤,如常见的导致功能活动严重受损的髋部骨折。
      • Abstract Not only do pollutants, like dust particles, H2S, COS, NH3, HCl and gaseous state alkaline metals, as contained in coarse coal gas, foul the environment, but they erode and abrade gas turbine buckets in addition.
        粗煤气中含有的粉尘、H2S、COS、NH3、HCl及气态碱金属等污染物不仅污染环境,而且严重磨损和磨蚀燃气轮机的叶片。
      • Q32 series abrade cleaning up machine has the advantages of advanced design, reasonable structure small energy consumption and high efficiency.
        是大、中、小型清理工部的理想清理设备。Q32系列履带抛丸清理机具有设计先进,结构合理,耗能小,效率高等优点。
      • Analysis on the principle of metal friction and abrade wear
        金属摩擦磨损机理剖析
      • Abrade mechanisms of Ni-P alloy coating are mainly adhesive wear, abrasive wear, fatigue wear and oxidative wear, while those of Ni-P-PTFE composite coating are mainly abrasive wear and fatigue wear, not including adhesive wear.
        Ni-P合金镀层的磨损机制主要有粘着磨损、磨料磨损、疲劳磨损及氧化磨损,Ni-P-PTFE复合镀层则基本不出现粘着磨损,主要是磨料磨损和疲劳磨损。
      • Dusr extraction metal hose is with high flexibility, low temperature resistant, hard to abrade and twist.
        吸尘软管韧特强,耐低温、耐磨损、耐扭曲;
      • All Meguiar's waxes are non-abrasive, this means Meguiar's waxes contain no ingredients that will abrade the paint or instill a scratch.
        所有的美光的蜡都是非研磨性质的,它不含可能磨损车漆或制造潜划痕的污染成分。
      • Take crural abrade medicine and skin allergy medicine to you can defer the advent of female menstruation?
        服用脚擦伤药及皮肤过敏药会不会推迟女性月经的来临?
      • Without delicate internal components to break, abrade or corrode, the Lake flow transmitter will provide many years of low-maintenance service.
        微妙的内部元件没有打破,研磨或腐蚀,湖流量变送器将提供低维修服务多年。
      • Especially, when abrade hard and brittle materials, ultrasonic abrasive could easily realize ductility removing. Therefore the processing surface is hardly ruptured, and high shape precision and low surface roughness is achieved.
        特别是在研磨硬脆材料时,超声波研磨易于实现脆性材料的延性去除,加工表面不易产生裂纹,能达到很高的面形精度。